  • Non or partial fill
     
    Possible Fault Cause Solution

    Metal temperature incorrect

    Increase metal temperature first before increasing the flask temperature (see burnout section).

    Flask temperature incorrect

    Increase flask temperature (see burnout section).

    Incorrect feed / sprue system

    Feed or gate should be attached to the thickest part of the casting. It should be at least 25% of the thickness of the casting.

    Insufficient centrifugal force

    Increase torque first and then RPM of the centrifugal casting machine. Only increase by small amounts each time (5%).

    Low vacuum when vacuum casting

    Change oil in pump on a regular basis. Check seals for blockages in the vacuum pipes.

    Not enough over pressure

    Only increase over pressure by small amounts each time (5%).

     
  •